Publication:
Sintering effect on mechanical properties of composites of bovine hydroxyapatite (BHA) and Li2O

dc.contributor.authorOKTAR, FAİK NÜZHET
dc.contributor.authorPEKER, İSMAİL
dc.contributor.authorGÜNDÜZ, OĞUZHAN
dc.contributor.authorSALMAN, SERDAR
dc.contributor.authorGENÇ, YUNUS EMRE
dc.contributor.authorsOktar F.N., Demirer M.R., Gunduz O., Genc Y., Agathopoulos S., Peker I., Ozyegin L.S., Salman S.
dc.date.accessioned2022-03-15T01:55:36Z
dc.date.accessioned2026-01-10T17:42:02Z
dc.date.available2022-03-15T01:55:36Z
dc.date.issued2006
dc.description.abstractIn this study, hydroxyapatite (HA) material, obtained from calcinated bovine bone (BHA), was mixed with 0.25, 0.50, 1.00, and 2.00 wt% Li 2CO3. The pressed pellets were sintered at various sintering temperatures between 900°C and 1300°C. Measurements of compression strength, microhardness, and density, along with SEM observation and X-ray diffraction analysis were performed. The experimental results showed that the samples with 0.25 and 0.50% Li2CO3. reached a maximum of densification and the highest values of compression strength and microhardness were achieved after sintering at 1300°C. The wetting effect of a Li2O-associated glassy phase was observed even from 900°C.
dc.identifier.doi10.4028/0-87849-992-x.49
dc.identifier.issn10139826
dc.identifier.urihttps://hdl.handle.net/11424/246756
dc.language.isoeng
dc.publisherTrans Tech Publications Ltd
dc.relation.ispartofKey Engineering Materials
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectBovine Derived Hydroxyapatite
dc.subjectLithium Oxide
dc.subjectMechanical Properties
dc.subjectSintering
dc.titleSintering effect on mechanical properties of composites of bovine hydroxyapatite (BHA) and Li2O
dc.typeconferenceObject
dspace.entity.typePublication
oaire.citation.endPage52
oaire.citation.startPage49
oaire.citation.titleKey Engineering Materials
oaire.citation.volume309-311 I

Files