dc.contributor.authorsOktar, FN; Genc, Y; Goller, G; Erkmen, EZ; Ozyegin, LS; Toykan, D; Demirkiran, H; Haybat, H
dc.contributor.editorMandal, H
dc.contributor.editorOvecoglu, L
dc.date.accessioned2022-03-12T15:58:58Z
dc.date.accessioned2026-01-10T16:51:42Z
dc.date.available2022-03-12T15:58:58Z
dc.date.issued2004
dc.description.abstractHydroxyapatite (HA) is a particularly attractive material for bone and tooth implants because of its chemical and crystallographic properties, which closely resemble those of bone and tooth minerals. Moreover, sintered HA material has superior biocompatibility. In this study, the compacts made of pure HA (Merck) were sintered at 1000, 1100, 1200 and 1300degreesC. The density, microhardness and compression strength tests were performed, in order to find out the optimum sintering temperature. As a result, average density was 2.554 +/- 0.37 g/cm(3), average compression strength value was 25.22 +/- 12 MPa and average value of Vickers microhardness was found as 250 +/- 120 HV (kg/mm(2)).
dc.identifier.doi10.4028/www.scientific.net/KEM.264-268.2087
dc.identifier.isbn0-87849-946-6
dc.identifier.issn1013-9826
dc.identifier.urihttps://hdl.handle.net/11424/224238
dc.identifier.wosWOS:000223059700501
dc.language.isoeng
dc.publisherTRANS TECH PUBLICATIONS LTD
dc.relation.ispartofEURO CERAMICS VIII, PTS 1-3
dc.relation.ispartofseriesKEY ENGINEERING MATERIALS
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjecthydroxyapatite
dc.subjectsintering
dc.subjectcompacts
dc.subjectmechanical properties
dc.subjectMECHANICAL-PROPERTIES
dc.subjectCOMPOSITES
dc.subjectCERAMICS
dc.titleSintering of synthetic hydroxyapatite compacts
dc.typeconferenceObject
dspace.entity.typePublication
oaire.citation.endPage2090
oaire.citation.startPage2087
oaire.citation.titleEURO CERAMICS VIII, PTS 1-3
oaire.citation.volume264-268

Files