Analysis of in-vitro reaction layers formed on plasma sprayed bioglass-titanium coatings

dc.contributor.authorsGoller, G; Yazici, T; Oktar, FN; Demirkesen, E; Kayali, ES
dc.contributor.editorMandal, H
dc.contributor.editorOvecoglu, L
dc.date.accessioned2022-03-12T15:58:49Z
dc.date.accessioned2026-01-10T19:45:36Z
dc.date.available2022-03-12T15:58:49Z
dc.date.issued2004
dc.description.abstractBioglass, 45S5 containing 45% SiO2, 6% P2O5, 24.5%, CaO and 24.5% Na2O all in weight percent, was plasma sprayed onto a titanium substrate with and without 60Al(2)O(3) 40TiO(2) as a bond coating. It has been observed that there is a uniform coating layer with a thickness of 110 mum and that there was not any reaction observed at the coating-metal interface for both coating application. In vitro assessment of bio-activity was carried out by immersing in Simulated Body Fluid (SBF). Fourier transform infrared spectroscopy and thin film X-ray diffraction techniques were used to analyze the inorganic carbonate apatite layer developed on coating in an in-vitro environment. Scanning electron microscopy was used to surface characterization.
dc.identifier.doidoiWOS:000223059700473
dc.identifier.isbn0-87849-946-6
dc.identifier.issn1013-9826
dc.identifier.urihttps://hdl.handle.net/11424/224173
dc.identifier.wosWOS:000223059700473
dc.language.isoeng
dc.publisherTRANS TECH PUBLICATIONS LTD
dc.relation.ispartofEURO CERAMICS VIII, PTS 1-3
dc.relation.ispartofseriesKEY ENGINEERING MATERIALS
dc.rightsinfo:eu-repo/semantics/closedAccess
dc.subjectbioglass
dc.subjectsimulated body fluid
dc.subjectBEHAVIOR
dc.titleAnalysis of in-vitro reaction layers formed on plasma sprayed bioglass-titanium coatings
dc.typeconferenceObject
dspace.entity.typePublication
oaire.citation.endPage1976
oaire.citation.startPage1973
oaire.citation.titleEURO CERAMICS VIII, PTS 1-3
oaire.citation.volume264-268